AUTOPLAY
Soldering Bezels To Ring With Tweezers
4 steps
Fluxing back of bezel plate, solder already flowed to flat spot on ring, set up in tweezers.
1. Fluxing back of bezel plate, solder already flowed to flat spot on ring, set up in tweezers.
1
Give enough tension to hold parts in place but not too much that if heated, back plate will sink.
2. Give enough tension to hold parts in place but not too much that if heated, back plate will sink.
2
Reflow solder that was pre-melted on the band in the flat spot.
3. Reflow solder that was pre-melted on the band in the flat spot.
3
Aligned bezel!
4. Aligned bezel!
4